Hemlock

Denominación científica:
Tsuga heterophylla Sarg.
Procedencia geográfica:
West Coast of North America
  • Sapwood: lightly whitter than heartwood.
  • Heartwood: light brown.
  • Fiber: straight and rarely wavy.
  • Grain: medium size to rough.
  • Characteristic defects: small lively knots.
Hemlock
a b c d e f g h i j k l m n o p q r s t u v w x y z
Impregnabilidad Propiedades mecanicas Mecanizacion logo Propiedades fisicas logo
Impregnabilidad
  • Sapwood: medium capacity of being impregnated.
  • Heartwood: low capacity of being impregnated.
Propiedades mecánicas
  • Resistance to static flexion 780 kg/cm2.
  • Elasticity module 108,000 kg/cm2.
  • Resistance to compression 450 kg/cm2.
Mecanización
  • Sawing process: easy with no difficulties.
  • Drying process: slow but easy to carry out, cracks and deformations are not frequent.
  • Planing process: no difficulties.
  • Gluing process: no difficulties.
  • Nailing and screwing process: no difficulties.
  • Finish: no difficulties.
Propiedades físicas
  • Apparent density at 12% humidity 480 kg/m3 light wood.
  • Dimensional stability
  • - Volumetric contraction coefficient 0.41 % stable wood.
  • - Relation between contractions 1.75% no tendency to deformity.
  • Hardness (Chaláis-Meudon) 1,4 softwood.
Observaciones
  • Ocasionalment pot presentar bosses de resina